Typical problems with brick and stone walls

Introduces common damage to brick and stone walls associated with unsuitable cement repairs and modern paint coatings.

Independent guidance from Heritage House 1 min read

Cement strap pointing causing massive damage to stonework by trapping moisture

Most problems you will see are in some way related to moisture. Where it is trapped into the structure, brick and stone will frass (split or spall) as included moisture is frozen.

Thick coats of masonry paint have soaked this wall to the point where it is disintegrating
A disintegrating brick wall, caused by thick layers of masonry paint and an injection 'damp course' that has allowed even more water into the walls through the drillholes. The lime mortar joints, the walls normal way of breathing and staying dry, are blocked with thick plastic paint. The entire wall, including mortar joints, is sodden. Removing the paint is the simple solution to drying it all out. Notice the dry patch around the second drill hole – this was the first bit of paint I removed – the rest we chopped off later. This dried in about 2 hours.
Stonework affected by plastic paint
Plastic masonry paint has prevented the stone door surround from breathing. Moisture has built up in the lime mortar joint, and is trying to escape – forcing the paint off around the joint – to the left you can still see bubbling paint – on the face of the stone is a wide band where the paint has been forced off by escaping moisture.